The sheet lies flat on the cutting bed. The profile looks clean, and the holes are where they belong. Then the last connection is released and one end of the shim rises. It is tempting to blame the final cut, but that moment may simply reveal a condition that was hidden while the surrounding sheet restrained the part.
Thin-shim distortion is not a single defect with one machine setting behind it. Local heating, stress already present in the stock, support during cutting and damage during removal can all leave similar-looking parts on the inspection bench. Separating those causes is more productive than repeatedly flattening the finished batch and hoping the problem disappears.
A clean edge and a flat part are different outcomes
Laser cutting concentrates energy in a small region. Good edge quality shows that the cutting process separated the profile acceptably; it does not, by itself, establish the final shape of the whole part. A narrow strip or a profile with long unsupported legs can respond differently from a compact blank cut from the same sheet.
SSAB’s explanation of thermal-cutting deformation distinguishes localized heating effects from the release of internal stress. It also notes the greater resistance to deformation provided by thicker material. Those mechanisms are useful when diagnosing a shim, although SSAB’s specific processing recommendations are written for its own steels and are not a universal thin-sheet recipe.
This is why “use less heat” is only a starting hypothesis. Cutting speed, energy delivery, contour order and material response must still produce a complete, acceptable cut. A change that reduces visible curl while leaving attached material or heavy edge deposits has moved the defect rather than solved it.
Observe when the shape changes
Inspecting only the final package makes it difficult to tell whether distortion came from cutting, release or handling. A more revealing trial records the part at several stages: while retained in the sheet, after release and cooling, after edge finishing, and after the intended cleaning and packing steps.
If the part lifts while still in the nest, investigate local heating, support and the order in which the remaining connections are removed. If it changes shape mainly when the final restraint is released, the stock condition and the release sequence deserve attention. If a previously flat part bends during separation or deburring, changing the laser program alone will not address the cause.
Use repeat trials with one controlled change at a time. Keep the material identity, sheet direction and part orientation in the record. A result obtained on one small coupon does not establish behavior for a long narrow shim with a different ratio of cut edge to remaining material.
A dense nest can be an awkward thermal neighborhood
Nesting optimizes material use, but adjacent cuts also affect the local process history. Several small profiles finished consecutively in one area can create a different condition from the same profiles distributed across the sheet. The sequence of internal features and outer contours changes how much surrounding material remains to support each operation.
Review that sequence with the actual geometry in view. Long slots, closely spaced cutouts and slender bridges deserve particular attention because the remaining material can become flexible before the part is complete. The objective is not simply a shorter program. It is a repeatable release of a part that still meets the drawing after it has cooled and left the bed.
The trial should also include the chosen material thickness and state. A successful route for a comparatively stiff spacer plate should not be assumed to work unchanged on thin shim stock.

Retaining the part solves one problem and creates another operation
Small connecting tabs can keep a profile attached while nearby cuts are completed. TRUMPF describes this purpose in its discussion of microjoint and nanojoint retention. The existence of retention technology does not mean every tab location is suitable for a functional shim.
A connection on a narrow leg may require awkward force to separate. A connection on a working edge may leave a local protrusion that affects seating. The removal operation therefore needs support and access of its own, followed by an edge and shape check. Twisting the part out of the skeleton can introduce a bend that was never present during cutting.
Agree where a connection may remain during processing and how the final contour will be restored. The companion article on thin-shim microtabs and removal positions looks at that design decision without treating a break-off mark as an acceptable default.
Define the inspection condition before deciding to flatten
A thin part placed on a surface plate can settle under its own weight or under a measuring probe. A part clamped between two plates may appear flat because the fixture forces it to conform. Neither observation alone describes the free-state shape. The drawing should distinguish a free-part requirement from an assembly condition with specified restraint.
If corrective flattening is proposed, evaluate it as a process step rather than a cosmetic rescue. Confirm that it does not damage the working faces, change the required dimensions or leave a result that depends on how the inspector holds the part. Recheck after the downstream steps that could alter the shape again.
For custom laser-cut shims and spacer plates, the practical route is to connect material selection, contour sequence, retention, edge finishing and final inspection. A profile that passes while still attached to a sheet is only an intermediate result. The part that matters is the one that reaches assembly, clean, released and checked in the condition the drawing actually requires.
Need a Custom Sheet Metal Quote?
Send us your CAD drawings — DRAmetal's initial response target is within 24 working hours. Quotation, DFM and lead-time timing depend on file completeness and engineering scope.
GET A FREE QUOTE →