A medical equipment drawing specifies Ra on a mounting face, while a supplier’s quotation promises an Rz value on the finished part. Neither document is necessarily unreasonable, but they do not yet describe the same acceptance condition. Treating them as interchangeable creates a dispute that is easiest to prevent before production.
Ra and Rz should be specified and evaluated as the actual parameters required, not converted using a convenient fixed multiplier. For formed sheet metal, the surface location and measurement conditions matter as much as the parameter name.
Resolve a parameter mismatch at RFQ review
Ra summarizes the average profile deviation; Rz describes a different aspect of the measured profile’s height characteristics under the selected standard. Their relationship depends on the surface profile, so one reported value does not establish the other. Mitutoyo’s surface roughness guidance explains parameter selection and the importance of measurement conditions.
If the drawing requires Ra, request Ra results. If the supplier recommends adding or changing a parameter, send that proposal to the design authority. Do not let purchasing accept a different symbol solely because the numbers look comparable.
Keep both requirements if the design genuinely needs both. In that situation, state whether every designated region must satisfy each limit and which procedure resolves a borderline result. A shared understanding is more useful than a loosely worded promise of a “mirror” or “medical” finish.

Define the regions that carry the requirement
A formed medical mounting plate can contain a broad flat face, an outside bend, hole edges and a locally blended weld. One instrument trace cannot be assumed to represent all of those areas. Mark the acceptance regions on the drawing or an accompanying inspection map.
Separate functional surfaces from cosmetic areas and from regions with different agreed criteria. If a limit applies to the outside bend, name that bend. If it applies only to the flat mounting face, do not leave the supplier to infer that from the part’s intended use.
The measurement plan should also state the manufacturing condition: before forming, after polishing or at final release. A raw-sheet result does not automatically describe a subsequently formed and finished component.
| Clause element | Information to release | Conflict it prevents |
|---|---|---|
| Parameter and limit | Required Ra, Rz or other specified parameter, with units | Substitution using a guessed conversion |
| Surface region | Identified face, bend or weld-adjacent zone | A convenient face representing the entire part |
| Measurement basis | Standard edition, filtering and evaluation settings | Different setups producing incomparable records |
| Direction and access | Agreed trace direction and usable measurement area | Unplanned measurement on the wrong feature |
| Sampling and decision | Parts, positions and acceptance rule | Averaging away a local nonconformance |
| Final condition | Relevant process stage and finish revision | Reusing an incoming-sheet result at final release |
Agree the measurement conditions, not just the instrument name
Ask for the proposed method before the first article is made. The inspection plan should identify the settings needed to reproduce the result, the surface direction and the available measurement length. Confirm instrument suitability and the practical means of supporting the part.
Two reports with the same units may still use different conditions. When results disagree, compare those conditions and locations before concluding that the finish changed. The guide to measuring near bends and welds addresses access constraints on formed parts.

Do not invent missing settings after a batch has been inspected. Record the gap and obtain an agreed inspection instruction. If a short feature cannot support the specified method, treat that as an engineering decision requiring approval, not a permission to shorten the trace without documenting it.
Separate process promises from measured acceptance
“Electropolished and passivated” identifies a route, not a complete roughness report. Specify the required final surface, then review whether the proposed fabrication and finishing sequence can deliver it without compromising thickness, fit or edge condition.
Likewise, a free-iron test is not a texture measurement. A finished part may need several independent acceptance checks. Keeping them distinct makes supplier comparisons clearer and prevents one certificate from being used to close unrelated requirements.
Close the specification before production release
Bring drawing notes, quotation exceptions and the first-article inspection plan into agreement. Where a customer accepts a limited deviation, identify the affected revision and quantity. Avoid allowing a one-time concession to become the undocumented requirement for future orders.

When requesting passivated stainless steel parts, include the surface map, required parameters, finish route and inspection deliverables. For terminology beyond this purchasing problem, refer to the surface-finish standards guide. The quotation should then state a measurable supply condition, not an assumed equivalence between Ra and Rz.