Choose shim materials around contact metals, moisture, load and surface protection. Compare stainless steel, carbon steel and brass for a defined joint.

DRAmetal Engineering Team November 2, 2026 5 min read
Stainless, Carbon Steel or Brass Shims? Start with the Contact Environment

A stainless shim can look like the obvious upgrade for a painted steel assembly. It resists rust, remains easy to identify and avoids a coating on the adjustment surface. Yet the joint contains more than the shim. If water reaches a damaged patch of the adjoining steel, changing only the shim material may move the corrosion problem rather than remove it.

Material selection therefore begins with the two contact surfaces, the loads passing through them and the environment trapped between them. Stainless steel, carbon steel and brass are not three levels of the same product. They have different mechanical and environmental roles, and an inexpensive piece of thin metal can alter the behavior of the much larger assembly around it.

Describe the joint before naming the alloy

Consider a hypothetical spacer between a machine bracket and a fabricated base. The same outline could be used inside a dry electrical enclosure, below a periodically washed machine, or beside an outdoor drain. Its geometry alone does not distinguish these conditions. Neither does a general note saying “industrial use.”

Describe whether the shim remains dry, sees condensation, receives cleaning chemicals or sits in a crevice that cannot drain. Identify both mating materials and their finishes. A shim against bare aluminum is a different interface from one against intact painted steel, even if the surrounding machine performs the same task.

Then identify what the shim must do mechanically. Does it carry sustained clamp load, establish a guide position, provide an intentional sacrificial contact, or set the height of a rotating machine? A material that is easy to trim during installation may be a poor choice where long-term dimensional stability under the specified contact pressure matters most. Alloy, temper and delivered condition belong in the decision, not just the family name.

Stainless steel does not make the entire interface stainless

Stainless is a useful candidate where the specified grade and surface condition suit the exposure. It should not be treated as immune to every chemical, cleaning method or confined wet joint. Outokumpu’s corrosion-resistance guidance distinguishes localized and galvanic mechanisms: dissimilar metals coupled in an electrolyte can behave differently from the same metals exposed separately.

For a shim, this means looking beyond the visible outer edge. Moisture can remain between closely contacting faces even after the surrounding equipment appears dry. Review drainage, crevice geometry, cleaning residues and whether the mating metal’s protective finish is interrupted. Selecting a more corrosion-resistant shim does not automatically protect that interrupted surface.

Electrical isolation may be part of an engineered corrosion-control solution, but inserting an arbitrary plastic film is not a neutral change. It introduces another material into the load path and may affect thickness, compression, temperature response or an intended electrical bond. The equipment designer needs to consider those functions together. A metal shim should also not be assumed to provide a qualified grounding path merely because it touches two conductive parts.

Stainless steel, carbon steel and brass shim pieces beside a metal mounting interface
Choose the shim for the complete contact pair and its exposure, not for appearance alone.

Carbon steel makes protection part of the thickness decision

Carbon steel may be appropriate for an approved dry, protected joint or a design with a specified protection system. The issue is not whether it can be used; it is whether the delivered and installed condition matches the intended environment. A bare cut edge, a disturbed coating and a clean metallic seating face are different conditions that should not disappear under a single “painted” description.

If the shim is plated or coated, state whether the thickness requirement applies before or after that process. A finish that is satisfactory on a guard can be unsuitable on an adjustment surface if its thickness or behavior under clamping has not been considered. Coating both faces changes the stack, while masking contact regions changes the corrosion-protection arrangement.

Protective oil also needs a defined role. Preservation during storage is not necessarily the intended final assembly condition. The cleaning method, permitted residue and re-protection of adjacent surfaces should be compatible with the joint. Avoid treating a bag of clean-looking pieces as proof that every surface is ready for final installation. The distinction between nominal and finished thickness becomes especially important when a secondary treatment is specified.

Brass deserves an application, not a blanket recommendation

Brass can be selected for particular interfaces, but its ease of cutting or conforming does not establish suitability under every clamped machine foot. The alloy and temper affect its behavior, and the bearing area matters as much as the total load. A narrow contact land can place demanding local pressure on a shim that appears generously sized from above.

For rotating-machinery alignment, SKF’s bearing maintenance handbook recommends suitable stainless sheet-steel machinery shims and cautions that inappropriate softer materials, including copper or brass, can deform and cause looseness. That guidance concerns machinery support; it is not a statement that brass has no legitimate engineering uses.

The practical consequence is to avoid changing a released steel shim to brass simply because brass is available or easier to adjust on site. Equally, replacing an intentionally specified brass contact piece with stainless can change the original design intent. Resolve the reason for the material choice before approving a substitution. Where the actual problem is motor soft foot, diagnose the support condition rather than seeking a material that will squash into the gap.

Keep the final choice attached to a condition

A useful selection statement names the material specification, condition, contact pair, protection system and service exposure. It also identifies whether material substitution requires approval. That gives purchasing and manufacturing something more precise than “corrosion-resistant shim,” without pretending that a single alloy solves every installation.

For custom metal shims and spacer plates, the resulting drawing should connect material choice to the finished thickness, contact area and edge condition. Confirm any special stock condition or surface treatment during review. The goal is not to buy the most prestigious metal; it is to preserve the intended gap and support relationship throughout the actual operating environment.

Need a Custom Sheet Metal Quote?

Send us your CAD drawings — DRAmetal's initial response target is within 24 working hours. Quotation, DFM and lead-time timing depend on file completeness and engineering scope.

GET A FREE QUOTE →
DRAmetal Engineering Team

Team-authored manufacturing guidance. Scope, sources, corrections, and project-status labels follow our engineering content policy.